This research presents the development and characterization of an innovative CoNi basedhigh entropy superalloy optimized for Laser Powder Bed Fusion L PBF technology Leveraging principles of high entropy alloys HEAs , the alloy composition comprisingCo, Ni, Cr, Al, V, Ti, Ta, and W is tailored to meet the rigorous demands of sustainableapplications Through a systematic investigation of process parameters, a processwindow is established to achieve parts with superior mechanical properties, includingtensile strength exceeding 1 GPa and ductility exceeding 30% at room temperature in asbuiltcondition Additionally, compression tests reveal remarkable yield strengthretention up to 700°C Microstructural analysis based on EBSD and TEM confirms theformation of a single phase fcc solid solution without any topologically close packed TCP phases and remarkable segregation, highlighting the alloy's crack resistant natureand high density achievable via L PBF The alloy's design principles, supported bycalculation of phase diagram CALPHAD using HEA database, underline its potentialfor high performance component production in critical industries
کلیدواژهها
نویسندگان
شیوه ارجاع
Mohammadzdeh, Ahad and De Nardi, Alessandro and Mostafaei, Amir and Torralba, Jose Manuel,1402,Advancements in Laser Powder Bed Fusion of Non-WeldableSuperalloys: CoNi-Based High Entropy Superalloy,6th International Conference on Welding and Non Destructive Testing & 24th National Conference on Welding & Inspection & 13th National Conference on NDT & 2nd National Conference on Additive Manufacturing,Tabriz
ارائهشده در
مجموعه مقالات ششمین کنفرانس بین المللی جوشکاری و آزمایش های غیرمخرب، بیست و چهارمین کنفرانس ملی جوش و بازرسی، سیزدهمین کنفرانس ملی آزمایش های غیرمخرب و دومین کنفرانس ملی ساخت افزایشی2 اسفند 1402 · تبریز