The effect of substrate's heat treatment on microstructure and mechanical properties TLP bonding X-45 and FSX-414 cobalt based superalloys
In this study, a dissimilar joint of cobalt based superalloys X 45 and FSX 414 has been created under the standard heat treatment conditions with the…
Transient liquid phaseCobalt-based superalloyfist nozzle-stage